Tin-Plating Crystals
These crystals produce a bright plated finish PCB track and other copper alloys. The plating provides a highly solderable keying surface. Deposition rates of tin to tin of 1.5 to 2.0 microns in the first half hour and 3 to 4 microns in up to 2 hours can be achieved at an optimum room temperature. 5 litres of solution can be made by dissolving the crystals in water at 50°C, which is sufficient to cover 2.7m2 of board. Instruction leaflet supplied.